2026-11-23
Anchor bolt edge distance is a centre-to-edge dimension, and the tape on site usually measures something else. A 50 mm clear gap between hole and concrete face converts to 56 mm centre-to-edge on an M12, which is 4 mm short of the 60 mm an assessment document asks for at hef 40 mm, and that shortfall is the difference between a fixing that holds and a concrete edge breakout. What follows gives the three measuring conventions, the corner case, the spacing rule, and the checks to run in the last minute before the bit turns.
Anchor bolt edge distance is quoted from the centre of the anchor to the free edge, so a clear-edge measurement compared against that figure overstates the margin by half the diameter.
Assessment documents state a minimum centre-to-edge distance, normally 1.5 hef. That is the number on the drawing and the number a design check uses, and it is measured to the axis of the anchor, not to the wall of the hole.
On site the tape normally starts at the hole edge, which yields a clear edge. The two figures differ by d/2 and nothing more, yet at small diameters the gap is wide enough to matter at the margin.

| Size | d (mm) | Centre-to-edge at hef 40 mm (mm) | Clear-edge equivalent (mm) |
|---|---|---|---|
| M6 | 6 | 60 | 57 |
| M8 | 8 | 60 | 56 |
| M10 | 10 | 60 | 55 |
| M12 | 12 | 60 | 54 |
| M16 | 16 | 60 | 52 |
| M20 | 20 | 60 | 50 |
Every size in that table is one of the concrete anchors we sell, so the d/2 gap applies across the whole range.
One case shows how the error lands. A crew measures 50 mm from the hole edge on an M12 and reports that the edge condition is met, because 50 mm looks close to the 60 mm on the drawing. Converted to a centre distance, 50 mm clear equals 56 mm, which is 4 mm short of the 60 mm required at hef 40 mm.
Treat a layout as compliant only when the centre-to-edge figure reaches 1.5 hef. A clear-edge figure that reaches the same number is d/2 short of it.
Two free edges govern at a corner, and the stricter of the two decides whether the fixing is usable.
Both directions carry their own 1.5 hef requirement, because the breakout surface runs out of concrete on whichever side is nearer. The cone is truncated there, so the volume resisting uplift shrinks even when the other direction is generous.
Failure at a corner shows up as concrete edge breakout, with spalling starting at the nearer face rather than around the anchor head. That signature tells you the fixing was placed too close to a free edge.

Averaging the two distances is not a permitted shortcut, and measuring diagonally to the nearest corner is not either. The governing distance is the shortest perpendicular from the anchor axis to a free edge, taken separately for each direction.
Mark both free edges on the layout before the point is fixed, and the direction that fails shows up while the drawing can still change.
Anchor spacing is a centre distance too, and the baseline is 3 hef.
At hef 40 mm that puts the minimum centre distance at 120 mm. Below 3 hef the two anchors share one failure surface, so neither can be counted as a single anchor with its own cone; the group is assessed as a group.

A second limit comes from drilling rather than from concrete mechanics. Two holes placed so close that only a thin web remains between them lose that web during drilling, and the expansion element then bears on a broken wall instead of a drilled one. Hole diameter and the minimum clear web between adjacent holes are not published on this site, so both come from the installation instruction for the model.
Group layouts go wrong when the average is checked instead of the minimum. Four anchors at 150 mm apart with one pair at 105 mm are not a 150 mm group. The 105 mm gap sets the group’s spacing, and the other three gaps stop deciding anything.
List every centre distance in the group, not the typical one, and compare the smallest against 3 hef.
Five moves exist once a layout fails, and they are not equal in cost or in what they disturb.
| Move | When it works | What it costs |
|---|---|---|
| Reduce hef or step down a diameter | the edge is fixed by the member and cannot move | capacity has to be recalculated, though 1.5 hef falls with it, so the edge condition eases |
| Change the layout | the connection plate can be redrilled | new plate, new coordinates, one round of approval |
| Change the anchor type | the edge is thin and a bonded or through-bolted fixing is available | longer setting sequence, different inspection |
| Enlarge the section locally | the member is still in design | structural change and a fresh check |
| Move the fixing point | the attachment has freedom to relocate | design revision and coordination with other trades |
The order of attempts runs layout first, product second, structure last. Layout changes cost a drawing; product changes cost a recalculation; structural changes cost a review.
A shorter wedge anchor at the same diameter lowers 1.5 hef, which is often the cheapest way back to a compliant edge.
Take the cheapest move that satisfies the edge condition, and record which one was taken on the revision.
Five checks in a fixed order catch nearly every edge and spacing problem, and each one stops the work if it fails.
A topping layer is what makes step two decisive. Even 20 mm of it moves the surface the tape should start from, and on a slab edge it eats 20 mm of the distance between the anchor and the free edge.
Run the five in order and write the four confirmed values on the work instruction, so the next shift inherits the numbers rather than the habit.
Five measurement errors repeat on site, and every one of them is detectable before the drill goes in.
Starting the tape at a formwork edge or a chamfer gives a distance longer than the structural edge allows, and the error is invisible on the sheet.
Reporting a clear edge as though it were a centre distance costs d/2, which is 5 mm on an M10 and 10 mm on an M20.
Ignoring a topping or levelling layer moves the real surface, and with it the point from which every dimension should have been taken.
Checking one direction at a corner leaves the other free edge unverified, which is precisely the direction that governs.
Measuring the net gap between two holes and comparing it with a centre-distance requirement pushes the number the wrong way. A net gap is always smaller than the centre distance by roughly one diameter, so a compliant group reads as failing on paper and a failing one can be argued into passing.
Pick the convention once, write it in words on the drawing, and four of the five disappear.
A layout drawing that names its measuring convention prevents the argument that otherwise happens at the wall.
| Item on the drawing | What it prevents |
|---|---|
| anchor centre coordinates, taken from the structural edge | offsets inherited from formwork or finishes |
| edge distance with the convention stated, centre-to-edge | the d/2 argument on site |
| anchor spacing as centre distances | net-gap readings substituted for spacing |
| member thickness at each fixing | an edge that exists on paper and not in the slab |
| concrete strength and crack state | a model quoted from the wrong qualification |
| the assessment document reference for the model | a depth and an edge value with no source |
Six lines turn a sketch into an instruction. The fourth is the one engineers most often leave to the site, and it is the one that decides whether a thin slab can carry the edge distance at all.
The same six lines apply to anything on the product list, not only to concrete anchors.
The limit belongs to the model, not to the diameter. Assessment documents state a minimum centre-to-edge distance, usually 1.5 hef, so a deeper anchor needs more edge. No page on this site publishes that figure for a specific model, so it has to come from the document or from the quotation.
Documents state it from the centre. Crews usually measure from the hole edge, which gives a value smaller by d/2. Both can be right, but only one can be compared against the document’s figure, and the drawing should say which.
Yes, and the edge requirement falls with it. A smaller hef lowers 1.5 hef, so a shorter anchor can fit where a longer one could not. The trade is capacity, which has to be recalculated rather than assumed.
They do once the centre distance falls below 3 hef. At hef 40 mm that baseline is 120 mm, so a 100 mm pair sits inside it and the group has to be assessed together rather than as two separate anchors.
Because the breakout surface has no concrete on the free side. The cone is cut off at the edge, so the resisting volume is smaller there than around the anchor head, and concrete edge breakout becomes the governing failure before pull-out does.
Anchor bolt edge distance ends up as one tape reading taken from the right line. Send the model code and the six drawing lines to whoever sets out the work, and the edge condition gets checked before the holes are drilled rather than after.