2026-11-23
Maɗaukakin ƙwaƙƙwarar ƙarfin ƙulli shine sakamakon gwaji da aka bayyana azaman ƙarfi, yayin da lambar da aka buga kusa da ita akan takaddun shaida ɗaya kayan abu ne da aka bayyana azaman damuwa. Takaddun shaida sun zo tare da adadi na MPa uku da takamaiman bayani, kuma jujjuya zuwa kaya yana buƙatar ƙima ta lissafi takardar shaidar ba ta cika bugawa ba. Karanta wannan kuma zaku iya jujjuya lambobi uku zuwa kiloewtons, gaya wa wane layi ne ya yanke shawarar karɓa, kuma ku ga takardar shaidar da ba ta cika ba kafin jirgin ruwa.
Lambobin guda uku akan takardar shedar ƙarfi mai ƙarfi sune damuwa a MPa, kuma babu ɗayansu mai nauyi.
Sp shine ƙarfin shaida (danniya dole ne a ɗauka ba tare da ɗaukar saiti na dindindin ba). ReL shine ƙananan ƙarfin amfanin gona, inda nakasar filastik ke farawa. Rm shine ƙarfin ƙarfi, mafi girman damuwa kafin karaya.
Damuwa uku, oda daya. Takaddun shaida mai inganci yana karanta Sp a ƙasan ReL a ƙasan Rm, saboda kullin da ke fitowa kafin ɗaukar nauyin hujja ya riga ya gaza manufar gwajin. Ƙimar daga cikin wannan tsari, ko kuma bacewar Sp, sun gaza yin rajistan farko kafin kowane lissafin ya gudana.
Karfe da bakin karfe ba sa raba teburi. Bolts a cikin azuzuwan 4.8 zuwa 12.9 ana rufe su ta ISO 898-1, yayin da maki A2-50 da A4-80 marasa ƙarfi suna bin jerin ISO 3506. Shafin DIN933 akan wannan rukunin yanar gizon ya lissafa iyalai biyu na kayan abu a layi ɗaya, wanda shine daidai inda takaddun takaddun guda biyu ke haɗuwa.
Bincika tsari na adadi uku da farko. Idan sun kasance daga jerin, babu abin da ke buƙatar ƙididdiga.
Wurin danniya mai jujjuyawa shine kawai mai ninkawa wanda ke canza MPa zuwa kN, kuma ba shine yanki na diamita na ƙididdiga ba.
Ƙimar ita ce As,nom = π/4 × (d - 0.9382P)², inda d shine diamita na ƙididdiga da P da farar. Rage lissafin sigar zaren: sashin ɗaukar kaya yana zaune a cikin zaren kuma ya yi ƙasa da cikakken da'irar.

| Girma (m) | Pitch P (mm) | Wurin damuwa na tensile As,nom (mm²) |
|---|---|---|
| M8 | 1.25 | 36.6 |
| M10 | 1.50 | 58.0 |
| M12 | 1.75 | 84.3 |
| M16 | 2.00 | 157 |
| M20 | 2.50 | 245 |
| M24 | 3.00 | 352 |
| M30 | 3.50 | 561 |
Yin amfani da πd²/4 a maimakon haka kuskure ne na gama gari a cikin bitar takardar shaida. Don M12 wanda ke ba da 113 mm² akan daidai 84.3 mm², yanki 34% yayi girma kuma saboda haka hujja tana ɗaukar na uku mai girma.
Pitch yana canza amsa ba tare da canza diamita ba. Zaren M12 mai kyau a farar 1.25 mm yana ba da 92.1 mm² tare da 84.3 mm² don ƙaƙƙarfan sigar, don haka ba za a iya duba takardar shaidar da ta jera diamita ba tare da farar farar ba.
Kowane girman da ke cikin wannan tebur shine madaidaicin girman girman, da kuma zangon kusoshi ana sayar da diamita da tsayi maimakon ta wurin damuwa.
Karanta d da P a kashe takardar shaidar, sake ƙididdigewa Kamar yadda, kuma kwatanta sakamakon tare da adadi da injin karfen da aka yi amfani da shi.
Nauyin hujja shine sakamakon gwaji; Ƙarfin yawan amfanin ƙasa shine kayan abu, kuma su biyun suna fitowa daga hanyoyi daban-daban.
Gwajin lodin hujja ya shafi Sp × Game da abin da aka gama, ya sake shi, kuma yana auna ragowar elongation. Kullin yana wucewa lokacin da ya dawo zuwa tsayinsa na asali a cikin juriya na daidaitattun abubuwan da aka tsara, wanda shine dalilin da ya sa gwajin ya zama wucewa ko gazawar hukunci maimakon lamba.
Adadin abin da aka samu ya fito ne daga gwajin ƙwanƙwasa da aka ɗauka zuwa lalata, inda lanƙwan-ɗorawa-ɗorawa ya faɗi. Yana siffanta karfe, ba ƙulli na mutum ɗaya ba, kuma an ruwaito shi azaman ƙimar da ba a haɗe hukunci ba.
Gwaji na uku yana kama yanayin rashin nasara na huɗu. Inda ma'aunin ya yi kira ga gwajin ɗora nauyi, an ɗora kullin ta hanyar wani yanki mai karkata a ƙarƙashin kai, kuma takardar shaidar da ta tsallake ba ta rufe kai ko gazawar shank maimakon gazawar zaren.
Takaddun shaida da ke karanta "nauyin hujja ya wuce" don haka bai ce komai ba game da adadi na ReL da aka buga a gefenta, kuma takardar shaidar da ke faɗin ReL ita kaɗai ba ta nuna nauyin hujja ba.
Nemo jumlar hanyar gwaji akan takaddun shaida kafin karɓar kowane bayani.
Ana iya karanta takardar shedar ne kawai idan filayen da suka dogara da juna suna nan, kuma tara daga cikinsu sun zama sarka ɗaya.
| Filin | Abin da ya ɓace idan ba ya nan |
|---|---|
| daidaitaccen lamba da bugu | Ba za ku iya sanin teburin da iyaka ya fito ba |
| ajin dukiya | babu darajar tunani da za a kwatanta da ita |
| mara iyaka diamita | Kamar yadda ba za a iya lissafta ba |
| rawa | Kamar yadda ba za a iya lissafta don zare mai kyau ba |
| zafi ko tsari lamba | ba za a iya ɗaure takardar shaidar da kusoshi a cikin akwatin ba |
| Sp | Ba za a iya yin hukunci akan nauyin hujja ba |
| ReL | Ba za a iya tabbatar da da'awar yawan amfanin ƙasa ba |
| Rm | ba za a iya tabbatar da da'awar karaya ba |
| hanyar gwaji da dakin gwaje-gwaje | sakamakon ba shi da hanyar da za a iya ganowa |
Sarkar tana gudana daga tsakiya zuwa waje. Diamita da farar ba da As; Kamar yadda aka ninka ta Sp yana ba da nauyin hujja; daidaitaccen bugu yana yanke hukunci ko Sp da aka nakalto shine wanda ake buƙata a halin yanzu. Cire duk wata hanyar haɗin yanar gizo kuma sauran ta daina kasancewa ana iya dubawa, wanda shine dalilin da ya sa takardar shaidar da ke ɗauke da Rm kawai ba gajeriyar sigar cikakken ce ba ce daban.

Daraja akan takarda da maki akan kai dole suyi daidai. An buga alamar ajin kadara a kan ƙwanƙwasa inda girman ya ba da izini, kuma takaddun shaida na 10.9 kusa da kawunan da aka yiwa alama 8.8 gazawar takaddun shaida ne maimakon tambaya mai ƙarfi.

Ƙirga filayen guda tara, kuma ku ɗauki duk wata hanyar haɗin da ta ɓace a matsayin buƙatun sake fitowa maimakon cikakken bayani don bi daga baya.
Ƙaddamar da ajin kadara a kan ƙwanƙwasa ƙarfin ƙarfi yana ɗaga duk matsalolin uku kuma yana rage haɓaka, don haka ciniki ne maimakon haɓakawa.
| Ajin dukiya | Tabbacin ƙarfi Sp (MPa) | Rage yawan amfanin ƙasa (MPa) | Ƙarfin Tensile Rm (MPa) | Tsawaitawa bayan karaya (%) |
|---|---|---|---|---|
| 8.8 | 580 | 640 | 800 | 12 |
| 10.9 | 830 | 940 | 1040 | 9 |
| 12.9 | 970 | 1100 | 1220 | 8 |
Waɗannan su ne ƙimar kamar yadda aka tsara a cikin ISO 898-1, kuma yakamata a tabbatar da su a kan bugu na yanzu kafin a nakalto su a cikin takaddar siyayya.
Tsarin bayan teburin shine cinikin. Tsakanin 8.8 da 12.9 ƙarfin hujja ya tashi kusan kashi biyu cikin uku yayin da tsayin daka ya faɗi ta uku, kuma haɗin gwiwa wanda ke buƙatar kullun don shimfiɗawa da ɗaukar motsi ya rasa daidai wannan ƙarfin.
Class 12.9 yana kawo ƙarancin aiki wanda 8.8 baya yi. Electroplating wani babban ƙarfin kusoshi yana ɗauke da haɗarin haɓakar hydrogen, kuma ƙayyadaddun bayanai kan sarrafa shi da matakin yin burodi ko ta zaɓin wani shafi na daban. Shafin DIN933 ya lissafa electro-galvanized, black oxide, hot- tsoma galvanized da Ruspert, don haka dole ne a yarda da hanyar shafi kafin a gyara aji.
Matsayi mafi girma baya nufin mafi girman ƙarfin haɗin gwiwa da kansa. Ajin na goro, mai wanki, preload da wuraren tuntuɓar duk dole ne a bi su, kuma ƙwanƙwasa 10.9 akan goro mai matakin 8 ya motsa hanyar haɗin mara rauni maimakon cire shi.
The DIN933 hex bolt page ya lissafa nau'o'in ƙarfe na carbon guda huɗu, 4.8 zuwa 12.9, da A2-50 da A4-80, don haka yakamata a zaɓi aji ta abin da haɗin gwiwa zai iya jurewa maimakon ta mafi yawan adadin da ake samu.
Takaddun shaida yana amsa tambayoyi game da zafi ɗaya, kuma yana yin shiru akan wasu biyar waɗanda masu siye suka ɗauka ya rufe.
| Ba a kan takardar shaidar ba | Inda adadi ya fito a zahiri |
|---|---|
| ƙara ƙarfin ƙarfi ko preload | ƙayyadaddun shigarwa don haɗin gwiwa |
| gajiya rayuwa karkashin cyclic load | lissafin ƙira, ba takardar shaidar kayan aiki ba |
| shafi kauri da hydrogen hadarin | ƙayyadaddun tsari na shafi |
| iyawar haɗin gwiwa da aka haɗa | tsarin haɗin haɗin gwiwa |
| ɗaukar hoto na batches daga baya | takardar shaidar kowane zafi ko lambar tsari |
Layi na ƙarshe yana da mahimmanci a cikin siye. Ɗaya daga cikin takaddun shaida yana kwatanta zafi ɗaya. Bolts daga zafi na biyu suna ɗaukar alamar iri ɗaya da aji iri ɗaya, kuma har yanzu suna buƙatar takaddun nasu, wanda shine dalilin da ya sa aikin da ke neman "takardar shaida" yana samun wanda ke rufe ɗan ƙaramin abin bayarwa.
Kowane ɗayan waɗannan biyar yana cikin takaddun daban-daban da mai shi daban: ƙayyadaddun shigarwa, ƙididdige ƙira, takaddar aiwatar da sutura, ƙirar haɗin gwiwa da rikodin tsari. Nemi takardar shaidar abin da ya kunsa, kuma ku bi sauran huɗun ta hanyar mutanen da ke riƙe da su.
Abubuwa shida sun yanke shawarar ko za a iya bincika takardar da ta zo, kuma duka shidan suna cikin binciken maimakon a cikin ƙarar daga baya.
Amsa mai dauke da rm kadai ta amsa daya daga cikin shidan. Aika lissafin baya maimakon karɓar ƙimar da baza ku iya amfani da ita ba.
Abubuwa shida iri ɗaya sun shafi kowane kullin akan index samfurin, ba kawai zuwa DIN933.
A'a. Ƙimar hujja ƙarfi ne da aka yi amfani da shi a gwaji kuma a sake shi, tare da haɗe da hukunci. Ƙarfin da aka samu shine damuwa inda nakasar filastik ta fara, wanda aka ɗauka daga gwajin juzu'i mai lalacewa. Ƙaƙwalwa na iya wuce nauyin shaidar sa kuma har yanzu yana da ReL kawai 10% sama da danniya na hujja, wanda shine al'ada ga ajin maimakon kuskure.
Haɓaka Sp ta wurin damuwa mai ƙarfi. Don M12 m, Kamar yadda yake 84.3 mm², don haka 580 MPa yana bada 48.9 kN, 640 MPa yana bada 54.0 kN kuma 800 MPa yana bada 67.4 kN. Yi amfani da wurin damuwa, kar a taɓa πd²/4, ko sakamakon ya fito kusan sama da uku.
Domin sakamakon tensile shine lamba ɗaya mafi sauƙi don bayar da rahoto kuma mafi arha don gwadawa. Yana amsa tambayar karaya kuma ya bar tambayar lodin hujja a buɗe. Nemi Sp da ReL akan shafi ɗaya, ko ɗaukar daftarin aiki azaman bayanin abu maimakon rikodin karɓuwa.
Sai kawai bayan duba abubuwa uku: goro da azuzuwan wanki, da preload da haɗin gwiwa zai iya dauka, da kuma shafi hanya, tun da mafi girma ƙarfi kawo hydrogen hadarin da electroplating. Kullin yana ƙara ƙarfi, haɗin gwiwa ba ya bi ta atomatik, kuma maye gurbin yana buƙatar sa hannu maimakon nod.
A'a. Bakin azuzuwan suna bin jerin ISO 3506, azuzuwan ƙarfe na carbon suna bin ISO 898-1, kuma su biyun suna amfani da alamomi daban-daban don ra'ayoyi masu ruɓani. Wannan rukunin yanar gizon ya lissafta iyalai biyu akan shafin DIN933, don haka takardar shaidar dole ne ta bayyana wace takardar da aka saita akan sa.
Ana iya karantawa ne kawai da zarar an lissafta yankin damuwa, kuma yankin damuwa yana buƙatar filayen biyu waɗanda takardar shedar bakin ciki ta fita. Aika abubuwa shida tare da binciken, kuma takardar shaidar da ta dawo za a iya bincika layi ta layi maimakon ɗaukar kan amana.